1, suitable for zinc alloy plating, spray before oil removal treatment. 2, alkaline, containing zinc alloy protective agent, cleaning workpiece can restore the original luster.
Dose: 20-50g/L (The actual concentration depends on the work piece, which is the laboratory test index)
Operating temperature: 50-70℃ (the actual operating temperature depends on the condition of the workpiece, which is the laboratory test index)
Cleaning time: 1-8min (the actual reaction time depends on the condition of the workpiece, which is the laboratory test index)
1, suitable for rust, iron products in addition to wax and oil. 2, wax and oil removal speed, less consumption, economic.
Dose: 30-60g/L (The actual concentration depends on the work piece, which is the laboratory test index)
Operating temperature: 60-95℃ (the actual operating temperature depends on the condition of the workpiece, which is the laboratory test index)
Cleaning time: 1-8min (the actual reaction time depends on the condition of the workpiece, which is the laboratory test index)
1. This product is suitable for removing wax and oil from alloy and copper parts. 2, does not contain strong alkali substances, no damage to the workpiece, after cleaning work can restore the origi
Dose: 30-60g/L (The actual concentration depends on the work piece, which is the laboratory test index)
Operating temperature: 60-75℃ (the actual operating temperature depends on the condition of the workpiece, which is the laboratory test index)
Cleaning time: 1-8min (the actual reaction time depends on the condition of the workpiece, which is the laboratory test index)
1, suitable for steel, copper, alloy workpiece cleaning. 2, cleaning process, mild reaction, easy to control.
Dosage: 40-70g/L (The actual concentration depends on the work piece, which is the laboratory test index)
Operating temperature: normal temperature -45℃ (the actual operating temperature depends on the condition of the workpiece, which is the laboratory test index)
Cleaning time: 2-8min (the actual reaction time depends on the condition of the workpiece, which is the laboratory test index)
1, the oil removal speed is fast, the use of low temperature, for heavy oil about 40℃ can be cleaned very clean, if the oil is light, can be used at a lower temperature.2, the oil removal powder does
Dose: 30-60g/L (The actual concentration depends on the work piece, which is the laboratory test index)
Operating temperature: normal temperature -45℃ (the actual operating temperature depends on the condition of the workpiece, which is the laboratory test index)
Cleaning time: 2-8min (the actual reaction time depends on the condition of the workpiece, which is the laboratory test index)
1, suitable for alloy degreasing (oil removal) treatment. 2, fast degreasing speed, easy to use, with ultrasonic cleaning effect is better.
Dose: 30-80g/L (The actual dose depends on the condition of the workpiece, which is the laboratory test index)
Operating temperature: 60-80℃ (the actual operating temperature depends on the condition of the workpiece, which is the laboratory test index)
Cleaning time: 2-8min (the actual reaction time depends on the condition of the workpiece, which is the laboratory test index)
1 Suitable for iron, stainless steel, aluminum alloy, galvanized plate, aluminum plate and other surface plating, coating before oil removal treatment. 2 Can be used to soak, ultrasonic, spray and
Dose: 30-80g/L (The actual dose depends on the condition of the workpiece, which is the laboratory test index)
Operating temperature: normal temperature -70℃ (the actual operating temperature depends on the condition of the workpiece, which is the laboratory test index)
Cleaning time: 0.5-8min (the actual reaction time depends on the condition of the workpiece, which is the laboratory test index)
1, suitable for zinc alloy and copper plating, spraying phosphating before treatment. 2, does not contain strong alkaline substances, alkaline minimal, no damage to zinc alloy, after cleaning can r
Dose: 20-50g/L (The actual dose depends on the condition of the workpiece, which is the laboratory test index)
Operating temperature: 40-60℃ (the actual operating temperature depends on the condition of the workpiece, which is the laboratory test index)
Cleaning time: 2-8min (the actual reaction time depends on the condition of the workpiece, which is the laboratory test index)
1, suitable for zinc alloy and copper plating, spraying phosphating before treatment. 2, does not contain strong alkaline substances, alkaline minimal, no damage to zinc alloy, after cleaning can r
Dose: 20-50g/L (The actual dose depends on the condition of the workpiece, which is the laboratory test index)
Operating temperature: 40-60℃ (the actual operating temperature depends on the condition of the workpiece, which is the laboratory test index)
Cleaning time: 2-8min (the actual reaction time depends on the condition of the workpiece, which is the laboratory test index)